Burst Crack caused by rupture extending out ward for a central point.
Chain Porosity Porosity in linear alignment.
Chafing A rubbing action between parts having limited relative motion. To be interpreted as an action which produces a surface condition rather than as a description of a damage. See also “gall” or “scratch”.
Chatter Marks Waves or ripples on a machined surface, in the direction of the cut.
  • Caused by a loose or dull cutting tool, or a tool that is not rigidly supported.
Clearly separated Imperfections which are not touching when viewed with the unaided eye
Cluster Two or more imperfections, clearly separated which can be contained within a circle of the maximum diameter allowed circle shall be counted as one imperfection
Cold Shut Intermittent of continuous lines caused by unfused material.